000 01169nam a2200301 a 4500
008 100012s1989 xxka 00 eng d
020 _a0580172147
040 _aUKM
_erda
090 _aBSI 17
_bBS 4080 : Part 1 : 1989
245 0 0 _aSpecification for severity levels for discontinuities in steel castings.
_nPart 1.
_bSurface discontinuities revealed by magnetic particle flaw detection /
_cBritish Standards Institution
264 1 _aLondon, United Kingdom :
_bBritish Standards Institution,
_c1989
300 _a10 leaves :
_billustrations ;
_c30 cm.
336 _atext
_2rdacontent
337 _aunmediated
_2rdamedia
338 _avolume
_2rdacarrier
490 1 _aBritish standard ;
_vBS 4080 : Part 1 : 1989
650 0 _aDefects.
650 0 _aSurface defects.
650 0 _aNon-destructive testing.
_961375
710 2 _aBritish Standards Institution
830 0 _aBritish standard ;
_vBS 4080 : Part 1 : 1989
907 _a.b16875394
_b2021-09-02
_c2021-09-02
942 _c4
_n0
_kBSI 17 BS 4080 : Part 1 : 1989
949 _a10015017
990 _azear
991 _aKoleksi Dokumen
998 _at
_b2021-09-02
_cm
_da
_feng
_gxxk
_y0
_z.b16875394
999 _c654821