245 1 0 _aStress corrosion cracking behaviour of austenitic stainless steel in 3.5 Wt% natrium chloride solution
_h[article] /
_cHaftirman, Ahmad Syayuthi Abd Rahman and Mohd Firdaus Jaafar
260 _aPutrajaya :
_bKementerian Pengajian Tinggi Malaysia,
_c2010
500 _aPTSL : Koleksi Dokumen
700 0 _aAhmad Syayuthi Abd Rahman
700 0 _aMohd Firdaus Jaafar
710 1 _aMalaysia.
_bKementerian Pengajian Tinggi
773 0 _tApplied and pure science : directory of research projects fundamental research grant scheme (FRGS) phase 1/2006 [article]
_g2010, p.489-492